Dear
I agree with Laxman & Manpreet,
For root pass, PQR shall be of 13 mm min. thickness

On Fri, Jul 29, 2011 at 7:53 AM, manpreet <manpreetsin88@rediffmail.com> wrote:
Hi Yash,
 
The root pass has to be at least 1/2" thick (QW-2004.b) and will qualify upto 1" thick in production (because t=T if t>19.1mm QW-451.1), therefore look for a GTAW PQR with min. 13mm thickness.
 
Regards
Manpreet Singh
 
 


From: yash yagnik <yash2223@gmail.com>
Sent: Thu, 28 Jul 2011 14:59:04
Subject: [MW:11943] QW 200.4(b)
Dear All,
 
Can anybody give detail interpretation of this clause??
 
For example I am describing below mentioned problem.
 
I want to weld 100mm thick plate for use of Heat Exchanger with Impact requirement and with the help of multiple processes - Root GTAW followed by SMAW and SAW.
 
I already have three PQR of individual process with GTAW - Thck 10mm , SMAW - 25mm thk and SAW - 50mm thk. All are satisfying imapct requirement.
 
 
NOW Can I use prepare a WPS with supporting of this three PQR?
 
My Interpretation of this clause is as under:
 
I can prepare this WPS with the help of this three PQR but my WPS will be qualified for thickness of 10mm to 20mm hence I cannot use this WPS for intended job.
 
If I can have PQR of GTAW with plate thickness of 13mm I can use this PQR and range will be 13mm to 100mm as root run GTAW  PQR with thickness of 13mm or more will qualify for any greater thickness base material root run welding.
 
 
If my interpretation is wrong or any new ideas/views or Observations are there from you people i would like to understand it.
 
Thanks
 
Yash Yagnik
 
 
                                                   
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...