[MW:11967] RE: 11956] SMAW - Welding Electrode Holder

With this design the electrode or the holder will come in contact with the work and cause scarring of the surface, have your quality assurance find these areas and have the contractor rework the area. This will cost the contractor extra and they will see it is cheaper to replace the holder than to rework the scarred areas.

The holder being used is not a CE approved holder and provides the welder no safety while performing his job, have your safety people condemn the holder and offer to replace the holders for the contractor.

These are the only solutions I see.

 

 



Description: cid:_1_0600CFAC0600CD40002C9083C12578D4
THE FIRST CHOICE IN TANK CONTAINERS
David Stevenson

Technical Manager
Eurotainer US
5810 Wilson Road, Suite 200, Humble, Texas 77396

Phone 1-832-300-5019 (Direct)● Mobile 1-713-805-0192 ● Fax 1-832-300-5050
email: dstevenson@usa.eurotainer.com ● website: www.eurotainer.com

Description: cid:_1_0600E23C0600DFD0002C9083C12578D4
 Please consider the environment before printing this document



 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ash_Ish Soni
Sent: Wednesday, July 27, 2011 10:29 PM
To: materials-welding@googlegroups.com
Subject: [MW:11956] SMAW - Welding Electrode Holder

 

Dear Member,

 

I have come across to know that our contractor is using Welding Electrode Holder as per the attached photo. Contractor is big enough to force without standard, so, I am searching for any International Standard which helps to force them to replace this kind of Welding Electrode Holder with the Standard one, which all of you know.

 

I have come to know one standard - IEC - 60974 - 11, but that is only for Safety point of view, which is not enough.

 

Request for the help.

 

Thanks & Regards,

 

Ashish Soni.

Essar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...