[MW:11937] Re: Equivalent ASTM material for EN S275JR

Hello,
By recent experience i have had a confusion as the supplier
produced a equivalent comparision statement from a certain
manufacturer as A36 = 275 , but from my records from past work done
for a internationally reputed client i confirmed that the same was not
true. i have the following clear statement ..

A36 [ASTM A36 1994] general = Fe 360 B [ ISO 630 1995 ]plates&bars =
S235JR [ EN 10025 1995 ]plates & bars
and
S275 JR [ EN 10025 1995 ] plts & bars = Fe 430 B [ ISO 630
1995 ]plts &bars = Gr. 42 [ ASTM A572 1994 ] plts...

no mention of A36

All the same i would strongly advice you should make a
comparision of the chemical composition and all the Mechanical
properties for the steel as required by S275 JR depending on the
application before using the steel supplied

best regards
hepo

On Jul 24, 4:57 pm, "K.Babu" <kbabu...@gmail.com> wrote:
> Pramoth
>
> No code will give equivalent chart.
>
> It is eqiovalent to A36 , Pls refer any of mill manufacturers website (May
> be JFE )
>
> On Sat, Jul 23, 2011 at 8:16 PM, PRAMODH NAIR <pramodhnai...@yahoo.com>wrote:
>
> >   Experts,
>
> > Could you please give me the equivalent ASTM material for EN S275JR with
> > reference code document.
>
> > Regards
> > Pramodh
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.
>
> --
> Thanks & regards,
>
> K.Babu
> Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...