Yes ,
 
You need to follow Project Specification which has approved by the client ....Golden Joint required 100 % RT ,there is no code says anything in this case ......
 
Client has to give you that requirement and it is general practice ...
 
Suresh

On Mon, May 16, 2011 at 6:24 PM, Venkat Ramulu <cvramulu@yahoo.com> wrote:
Dear Experts,
Can any body clarify that,is it  pluss joint acceptable in piping, as per B31.3 or ASME ,if  100% RT taken. Pl give code referance.
 
Thanks and regards,
C.V.Ramulu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...