Re: [MW:11017] Difference Between IS 2062 Grade A & B

CARBO PERCENTAGE :GR A -0.23,GRB-0.22,GR C 0.20
WELDABILITY INCREASES FROM A TO C
Y GRROVE CRACKABILITY TEST ONLY FOR GR C.
IMPACT TEST IS NOT DONE FOR GRADE A

On Mon, May 9, 2011 at 3:48 PM, Ravi Karuskar <rkaruskar@gmail.com> wrote:
Dear Experts,

Pls. explain difference between IS 2062 Gr. A & Gr. B.

--
Ravi Karuskar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...