Monday, May 9, 2011

Re: [MW:11001] Re: 10934] AWS D1.1 WPS M.no changes requiring requalification or not?

Pls.refer Table 3.1

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Sun, 5/8/11, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:

From: Srinivas Engr <srinivas.gmsrini@gmail.com>
Subject: [MW:10997] Re: 10934] AWS D1.1 WPS M.no changes requiring requalification or not?
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Sunday, May 8, 2011, 5:59 PM

Dear All,

@ Babu & elumalai,
as from ur words,
AWS D1.1 says only on Group number.
&
In Table 4.5, PQR essential variable.
point 29) a change in base metal or combination of basemetal not
listed in pqr or qualified by table 4.8.
that means
Group number is the only essential variable here for base metal.
no other variable for basemetal.
am i right?

& G.no taable for material is not given in aws d1.1. where to refer
for that?

Regards
Srinivas


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...