[MW:11074] Query regarding Flanges

Dear experts,
 
                Our existing weldneck flange butt weld failed due to improper support provided and we decided to replace it. Now the existing one is SA182 Type F304L due to unavailability of this we decide to replace it with readily available SA182 Type  316L. PNO & GROUP NO remain same for both the flanges as per section IX.
 
 Is it compatible in terms of weldability and its intend service or what will be the consequences if its welded? or should we use only type F304L?
 
Can somebody explain me?
 
Regards
Ilangkumaran 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...