[MW:11023] RE: 11022] PQR with Impact test, Thick Qualified

See QW-451.1 

 

Without impacts assuming both base metal thickness and weld metal thickness, single process, are 9mm then per second line qualified base metal thickness range is 1.5mm to 2T or 1.5mm to 18mm and weld metal is qualified to a maximum of 2t or 18mm.

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Wednesday, May 11, 2011 9:42 AM
To: materials-welding@googlegroups.com
Subject: [MW:11022] PQR with Impact test, Thick Qualified

 

Hi all,

  I have one PQR 9 mm thick, with impact test. The range qualification of qualified WPS with Impact test is 9 mm to 16 mm according QW 403.6 .
My question is; What's the thick range qualification qualified by this PQR without impact test, where it's mention in ASME sect IX ?

Regards

--

زكرياء غراب
GHRAB Zakaria

مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...