[MW:11019] Impact test after simulation PWHT in PTC

Gents,

Is it acceptable to do Impact testing on PTC with simulated PWHT. In my opinion we are testing the coupon in worst condition. Pls provide your feed back.


Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.