Dear All Experts,
 
Ref Code: ASME Sec VIII, Div 1, latest Edition
 
Refer to UW-51 which states that a written Procedure is not required for Radiographic Examination.
Refer to UW-53 which states that a written Procedure is required for Ultrasonic Examination and shall be demostrated.
 
Query: As I understand that Radiography Examination is having predominate over UT Examination for all Pressure Vessel as per this division, but as per UW-51 it does not require any written Procedure. Why? I think it should be the vice versa. Please explain.
 
Addtion Question:
1. Do we require a UT Procedure to be demostrated for U-Stamp Pressure Vessel? If so, how to prepare a mock up and please provide a reference in ASME for preparation of mock-up.
2. What is the limitation of Pressure Boundry in Pressure Vessel? Is it the first welding ? Does further nozzle or pipe spool includes in the Pressure Vessel? Refer to Attachment.
 
Hope to see positive response from every end.
 
Thanks & Regards
Vino - Doha

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...