[MW:10982] ultrasonic acceptance and rejection criteria

sir
 
i want to know how to apply ultrasonic inspection acceptance and rejection criteria according to ASME and AWS D1.1
 
regarding to AWS D1.1 table 6.2 and 6.3 i cant understand what the numbers is table mean , i will be thankful if i get an answer
 
thanks and best regards