[MW:10960] RE: 10934] AWS D1.1 WPS M.no changes requiring requalification or not?

There is no " M" number in AWS D1.1. you need to refer the Table 3.1
(prequalified materials list.)

And Group II will cover Group I & II. Follow the table 4.8.

You can take any one material from Group II ,Table 3.1.

With Kind regards,

S.Elumalai.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Srinivas Engr
Sent: Tuesday, May 03, 2011 9:08 PM
To: Materials & Welding
Subject: [MW:10934] AWS D1.1 WPS M.no changes requiring requalification
or not?

Dear all,

as per table 4.5 essential variables..
in base metal, it says to refer table 4.8.
In table 4.8 it says about only group number.
if group number changes from one which is not qualified require
requalification.. ok.
My question is..
Its doesn't says about M.number. so m.no changes is not required
requalification of wps.
can we go with same WPS if g.no mets?
The above said is right or wrong..
clear me.

Reagrds
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
******************************************************************************************
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...