Friday, July 23, 2010

RE: [MW:6091] protocol used for Chemical analysis

Dear Sir

But ASTM E415 is applicable for Carbon & Alloy steel only. What about for Stainless Steel ?

 

Regards

Subrata Das

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Harish Kannepalli
Sent: Thursday, July 22, 2010 3:24 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6077] protocol used for Chemical analysis

 

Is astm e415

2010/7/22 subrata das <sdas@pkgroup.org>

Dear All

What are the standard protocol used for Chemical analysis of CS, AS & SS with Argon based spark ignition spectrometer as per ASTM-E / ASME  Standard.

 

Regards

Subrata Das

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





K Harish Kumar, MTech
Consultant for:
Corrosion Metallurgy
Failure Analysis Surface Coating
Thin Films Vacuum Systems QMS.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...