Dear Shibu,
 
Find the attached chart for Preheat requiremets, for the below query mention preheat temperature as min 50deg c in the WPS.
 
regards,

On Sat, Jul 17, 2010 at 9:08 PM, shibu simon <shibusimon2000@yahoo.co.uk> wrote:
Dear all,

Carbon steel base metal initial temperature was 32 deg celcius, during PQR qualification as per API 1104. Decreasing pre heat temperature is an essential variable as per API 1104. So what minimum preheat temperature to give in WPS.

Thanks.

shibu simon




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
G.Murali krishnan


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...