Hieee Pankaj,

Kindly check the argon gas purity and also check the purging is sealed properly or there is any leakage and air is entrapping inside. kindly check what is parent material , and welding consumable if the consumable is right for parent material. check all those parameters.

regards

shamesh lotlikar
welding consultant


From: pankaj abhang <pankaj.abhang1@gmail.com>
To: materials-welding@googlegroups.com
Sent: Fri, July 16, 2010 9:29:09 AM
Subject: Re: [MW:5992] Problem wk\hile root run

Check your fillerwire grade if GTAW if ok then chek its chemistry.
I think this problem is with your filler wire.
 
 
 
 
PANKAJ

On Wed, Jul 14, 2010 at 6:27 PM, waman nilesh <wamannp@gmail.com> wrote:
I have problem while doing root run the weld get black from backside as we have maintain the backing 10 lpm & Shielding 12 lpm as per WPS. 
Can anybody tell me the reason & how to avid it.

Nilesh 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...