Thursday, July 15, 2010

Re: [MW:5986] Problem wk\hile root run

change the purging to 6-8 ltr.
reduce the root gap 

Thanks & Regards
Muhammed Ibrahim PK



On 15 July 2010 10:27, waman nilesh <wamannp@gmail.com> wrote:
I have problem while doing root run the weld get black from backside as we have maintain the backing 10 lpm & Shielding 12 lpm as per WPS. 
Can anybody tell me the reason & how to avid it.

Nilesh 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...