The Flange face finishing is checked with visual comparators as per ASME B46.1. Which is clearly specified in ASME B16.5 Para 6.4.5.
Thanks & Regards,
Sajeev
On Mon, Jul 5, 2010 at 5:58 AM, James cyrilandrew <jcyrilandrew@gmail.com> wrote:
--
---------- Forwarded message ----------
From: James cyrilandrew <jcyrilandrew@gmail.com>
Date: Sun, Jul 4, 2010 at 5:37 AM
Subject: DOUBT-
To: Material welding groups <materials-welding@googlegroups.com>
Hi,I want to check the flange serration area. whether the machining microns is meeting the requirement. how to check .what is the instrument used. what is the standard to compare.thanks.Regards,J.Cyril AndrewsQatar
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment