Thursday, July 22, 2010

[MW:6063] FW: MW- 0- Welding of 140 KSI material


 

Romeo,

 

What’s the design code, what’s the materials of construction, piping thickness involved, is there any other client or  service specific requirements?

 

I strongly feel the above details or anything more you have would be essential in selection of welding process/consumables.

 

Appreciate your reply.

 

Thanks.

 

Pradip Goswami,P.Eng.

Welding & Metallurgical Engineer/Specialist

Ontario Power Generation Inc.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of romio dabre
Sent: Monday, July 19, 2010 1:10 AM
To: materials-welding@googlegroups.com
Subject: [MW:0] Welding of 140 KSI material

Dear All

 

We need to weld following pipe material

 UTS 845/855 Mpa,

 T.S. - 990/1000Mpa

 Chemical Comp. - 0.35C, 0.65Mn, 0.20Si, 0.95Cr., 0.18Mo

 

Can anybody advise suitable consumable for this application

 

Thanks

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...