Monday, July 5, 2010

[MW:5856] inconel 625 class: "REDUCED RATING BECAUSE OF USING A 453-660 BOLTS"

Dear all,
            I got 1 querry from my friend, i was unable to solve it.
For querry please refer below.
 
---------- Forwarded message ----------
From: Namita Aher <Namita.Aher@lurgi.com>
Date: Fri, Jul 2, 2010 at 6:59 PM
Subject: Fw: plz reply
To: gorantiwar.swapnil@gmail.com





I read the sentence in one of my pipe class of inconel 625 " REDUCED RATING BECAUSE OF USING A 453-660 BOLTS." plz explain...

i m attaching here the pipe class for reference....





FLUID : SHO IS





Namita A Aher
Piping Engineer
Lurgi India Company  Pvt. Ltd
A-24/10
Mohan Co-Operative Industrial Estate
Mathura Road.
New Delhi-  110044
Phone No. : 011 - 42595197
-



--
Best Regards,

Swapnil Gorantiwar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...