Sunday, July 4, 2010
[MW:5848] STRESS RELIEVING REQUIREMENT
Hello,
As per ASME B31.3; for CS material PWHT requirement is above 20mm.
Is this applicable to category D fluid service class also?
Or code has given liberty to skip PWHT for category D fluid service even though thickness is greater than 20mm.
Pls. advise.
Thanks in advance,
Thanks & Regards,
Dhwani Desai
Planning & Piping Dept.
Ext.-7681 --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34920] Tubesheet Hole step
Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP -- https://materials-...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment