Dear All,


We are try to weld a 5mm Strip to a tube of wall thickness 2mm Mild
Steel [ O_ ] In this position. We need to weld vertically and from
both sides at the same time front and back. Is it ok to do so ? Will
there be a problem if we weld both from front and back at the same
time ? Is it better to weld one side first then the other ? We are
using 1.0 mm solid wire and CO2 as gas.

Regards,

--
Nimesh S Chinoy

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...