[MW:3384] Re: R: 3361] Re: Heat Input

Dear Mr. Adi,

I don't understand about the combination selection of 6013 and 7018-1,
In LTCS with tensile strength more than 60 not suitable to do the
welding with 6010.

Regarding Heat input it depend upon your client specification and
Manufacturer's specification, Normally every manufacturer give the
limit of heat input depending upon the material and that heat input
should not be more than the manufacturer's specification.

You can get this value in catalog of material manufacturer.

On Sep 29, 11:42 am, Jeremy Zibin <jzi...@yahoo.com> wrote:
> Francesco,
>  
> I agree that the cellulosic electrode is problematic for low temp. applications, especially for danger of H2 cracking.  There is usually tight quality control on the electrodes and they are always in rod ovens prior to use.  Also, the root pass is limited in thickness, 5 or 6mm if I remember properly on the WPS, applied with a small diameter electrode.  The second pass (7018) or hot pass is applied immediately after the root pass and it blends in with the root pass and thus creates a mixture of 6010 & 7018 in the root (i.e. the root is not totally 6010 in mech. properties).
>  
> I'm just adding to the discussion what I've observed in the oil & gas industry in Canada.  The welding with 6010 & 7018 for LTCS is quite common and it is approved from very large clients at multi-billion dollar sites that have been in operation for 20 years or more, so I would think these people know their welding, especially in the cold temperatures of Northern Canada where it is not uncommon to see -50 or -60C during the Winter.
>  
> Of course a GTAW root would be of higher quality and shouldn't have any issues with low impact resistance but this process is impractical/uneconomical for production welding on construction sites where manual welders are welding hundreds or thousands of pressure piping joints everyday.  Not to mention, you would have trouble finding enough welders that could TIG roots on these large construction sites in the oilsands.
>  
> Regards,
>  
> JZ 
>
> --- On Tue, 9/29/09, Cotzia Francesco <Francesco.Cot...@saipem.eni.it> wrote:
>
> From: Cotzia Francesco <Francesco.Cot...@saipem.eni.it>
> Subject: [MW:3363] R: 3361] Re: Heat Input
> To: materials-welding@googlegroups.com
> Received: Tuesday, September 29, 2009, 1:13 AM
>
> Jeremy,
>  
> The use of cellulosic electrode for low temperature carbon steel is not quite appropriate. Sometimes and especially nowadays there some product classified as E6010 that can bear CVN at -46°C. I don't know the diameter of root pass electrode, the WT you have used for PQR nipple, but I think that the weld metal deposited by cellulosic electrode is not more than 2mm. When you are extracting the CVN specimens, you will never test them the root pass. Then you are not sure that the E6010 will resist at -46°C. This risk will be increased if you are using high heat input.
> If you are using this type electrode, you are increasing the risk to have hydrogen cracks especially in the root. I would suggest to use GTAW or low hydrogen electrode (E7016-1) for the root pass.
>  
> Regards
>  
> F
>
>  
>  
>  
>
> Da: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Per conto di Jeremy Zibin
> Inviato: martedì 29 settembre 2009 9.56
> A: materials-welding@googlegroups.com
> Oggetto: [MW:3361] Re: Heat Input
>  
>
> Gentlemen,
>
> We've used qualified welding procedure specifications for LTCS that specifiy a root layer of 6010 (but only 1 root layer and no hot-pass) and then fill and cap layers with 7018.  This welding was performed on pressure piping under B31.3 for use in Northern Canada (min. design temp. of -46C).  The WPS was qualified, stamped by professional welding engineers and approved by the client.
>
> It is my understanding that the root lay is limited in thickness on the WPS and therefore the total thickness and properties of the full weld are majority 7018, which is approved for LTCS.  The heat input is limited to a max. on the WPS so that the welded joint should have the adequate impact properties at low temperatures.  This will be proven during qualification but remember not to limit yourself on heat input on the WPS, use a typical heat input for your welding process and material thickness to pass the qualification.
>
>  
>
> Regards,
>
>  
>
> JZ
>
>  
>
> --- On Mon, 9/28/09, Muhammed Ibrahim <ibrat...@gmail.com> wrote:
>
> From: Muhammed Ibrahim <ibrat...@gmail.com>
> Subject: [MW:3358] Re: Heat Input
> To: materials-welding@googlegroups.com
> Received: Monday, September 28, 2009, 11:16 PM
>
> E6010 will support up to -29 degree celcius only and used in pipe line root application. But if the PQR passes the impact you can use it with batch restriction.
>
> regards,
>
> Ibrahim
>
> 2009/9/29 BHARAT GOLE <bharatg...@hotmail.com>
>
> E 7018-1 is acceptable up to -46 degree but selection E 6010 is not suitable for LTCS ! As per which clause it is selected for LTCS ?
>
> Regards
>
> Bharat B. Gole
>  
>
> Date: Tue, 29 Sep 2009 09:49:23 +0530
> From: nach_...@yahoo.com
> Subject: [MW:3354] Re: Heat Input
> To: materials-welding@googlegroups.com
>
> Adi,
>
> Heat input is a guideline for subsequent welding. The yardstick is the average  value as obtained from your PQR. Your production welding should not exceed PQR HI values.
>
> By the way, is 6010, 7018-1 Ok for LTCS?  What is the working temp?
>
> Shashank Vagal
>
> --- On Tue, 29/9/09, Adi <adinr...@gmail.com> wrote:
>
> From: Adi <adinr...@gmail.com>
> Subject: [MW:3352] Heat Input
> To: "Materials & Welding" <materials-welding@googlegroups.com>
> Date: Tuesday, 29 September, 2009, 9:35 AM
>
> I have done the PQR for LTCS by using 6010 & 7018-1 as per ASME SEC IX
> some time i got 5KJ heat in put
> What is the limitation for heat input and where it is mention?
>
> Adi
>
> From cricket scores to your friends. Try the Yahoo! India Homepage!</a
>
>  
>
> Get easy photo sharing with Windows LiveT Photos. Drag n' drop
>
>  
>  
>
> --
> Thanks & Regards
> Muhammed Ibrahim PK
>  
>
> Be smarter than spam. See how smart SpamGuard is at giving junk email the boot with the All-new Yahoo! Mail </a
>
>  
>
> *************************************************************************** ***************
> CONFIDENTIALITY NOTICE
> This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.
>
>       __________________________________________________________________
> Ask a question on any topic and get answers from real people. Go to Yahoo! Answers and share what you know athttp://ca.answers.yahoo.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...