Dear Mr. Azmi A pin hole of 5mm deep in a weld of only 6mm detected by visual examination is not accceptable. Gopu
--- On Mon, 28/9/09, asad azmi <azmiasadayub@gmail.com> wrote:
From: asad azmi <azmiasadayub@gmail.com> Subject: [MW:3338] ACCEPTANCE OF ROUNDED INDICATION BY VISUALL INSPECTION To: materials-welding@googlegroups.com Date: Monday, 28 September, 2009, 1:05 PM
GOODMORNING........... can anybody can confirm whether a pin hole of diameter 3mm and depth of approximately 5 mm in fillet weld of 6mm of material SA 516GR 70 can be VISUALLY accepted. The vessel is fabricated as per ASME SEC VIII DIV 1. If YES then by which code. Kindly note that if we consider acceptance crieteria for PT/MT, as per ASME SEC VIII DIV 1, APPENDIX 6/8, Rounded indication upto 4.8mm is acceptable. can the above defect can be accepted on the basis of acceptance crieteria of PT/MT. please reply ASAP. Thanks & Regards Asad Azmi
On Thu, Sep 24, 2009 at 1:35 PM, Adi <adinraos@gmail.com> wrote:
If joint repair came in 2" pipe, it is very difficult to identify repair the exact location & root repair we can't do, so the joint should be cut out My question is When we are calculating the welders repair % we have to consider total length of 2" is repair ? Why because we repaired the total length Is it correct please advice
Adi
Connect more, do more and share more with Yahoo! India Mail. Learn more --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-