E 7018-1 is acceptable up to -46 degree but selection E 6010 is not suitable for LTCS ! As per which clause it is selected for LTCS ?
Regards
Date: Tue, 29 Sep 2009 09:49:23 +0530
From: nach_sam@yahoo.com
Subject: [MW:3354] Re: Heat Input
To: materials-welding@googlegroups.com
Get easy photo sharing with Windows LiveT Photos. Drag n' drop
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Regards
Bharat B. Gole
Date: Tue, 29 Sep 2009 09:49:23 +0530
From: nach_sam@yahoo.com
Subject: [MW:3354] Re: Heat Input
To: materials-welding@googlegroups.com
| Adi, Heat input is a guideline for subsequent welding. The yardstick is the average value as obtained from your PQR. Your production welding should not exceed PQR HI values. By the way, is 6010, 7018-1 Ok for LTCS? What is the working temp? Shashank Vagal --- On Tue, 29/9/09, Adi <adinraos@gmail.com> wrote:
|
Get easy photo sharing with Windows LiveT Photos. Drag n' drop
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments