Wednesday, September 30, 2009

[MW:3375] RE: 3373] filler wire for copper

 

GTAW wire ''ERCu''

 

 

 

Regards,

Vasanth

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of gajjalla surya prakash
Sent: 30 September 2009 07:17
To: materials-welding@googlegroups.com
Subject: [MW:3373] filler wire for copper

 

 

dear all ,

 

can any one sujjest me the filler wire for GTAW process for weld 12mm

thk Pure copper to copper plate(99.3%)

 

--

With regards,

 

Surya Prakash Gajjalla

ASSOCIATED ENGINEERING SERVICES

3-5-944/220-221 panchavatimall narayanaguda hyderabad india 500029.

 

www.aesinspections.com

0091 9885162668

 

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...