Hello Norberto,
Normalised C – Mn steel.
Requirements reg charpy values can be till @ -40 degr.
Welding with E 7018 or E7018-1 like
TENACITO R or SUPERCITO 7018S
http://www.alw-tool.com/WPC/oerlikon/MA/EN/index.php


Met vriendelijke groet, with kind regards,
mit freundlichem Grüss, Salutations,
Ing. Erwin GERING, IWE
Product Manager Welding Consumables
Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Norberto Barbosa
Verzonden: vrijdag 25 september 2009 13:11
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:3317] Base Metal
Hi, everybody
Is there someone who knows this kind of Base Material "S-355 J2 G3", regarding;
1)Similarity with ASTM;
2) Quimical Composition
3) and if possible an adequate electrode with its AWS classification and specification to weld this material.
I'll be glad.
Regardings,
Norberto de Souza Barbosa - Brazil
Novo Internet Explorer 8: mais rápido e muito mais seguro. Baixe agora, é grátis!
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments