Dear
 
The problem is coming from inorganic primer which might be with more DFT.Either you have to control the DFT or during application of intermediate coat,first apply mist coat then followed by required DFT.Same procedure to be followed for top coat.This can resolved your problem due to escaped gases from primer during mist coat application.
 
regds

On Sat, Sep 26, 2009 at 12:46 PM, Saravanan Mohan <sardev@gmail.com> wrote:
Dear Guys!!!!!!!
 
The project which I am involved following the paint systems as per client spec follows:-
 
Inorganic Zinc(75-100 micron) as a primer
High Build Epoxy(100-150 micron) as a Intermediate
High Solid Aliphatic Polyurethane(40-100 micron) as a finish
 
Total Dft between (215-350 micron)
 
After the complete curing of the finish coat visually I observed tiny pinholes like appearance or fish eye only inspector eye can find them.
 
Please give me the suggestion where the problem from? this appear in almost all the painted works which applied many different days, different paint batch followed by airlesspray method.
 
 
 
 





--
Nilesh Parsekar
Sr QC Co-ordinator
Exterran Belleli Energy
Fujairah - Sidem
Mobile - 0506561785

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...