[MW:3309] Re: application of SS Flux cored wire for GTAW, SFA 5.22

Yes, STT is a good option only if you could use GMAW process. And its worth an investment only if such jobs are regular.

Besides STT, even Miller Electric has developed their patented technology RMD - Regulated Metal Deposition. Machine Model is Pipepro 450. Its somewhat similar to STT and a little more to offer. check www.millerwelds.com

Regards

VISHAL



On Fri, Sep 25, 2009 at 8:54 AM, vipin george <vipingeorges@gmail.com> wrote:
Dear Bathula,
 
A new process is developed by Lincoln STT(Surface tension transfer) it's GMAW process with short circuit transfer.It's good for piping applications.Check Lincol electric.

Regards,
vipin


On Tue, Sep 22, 2009 at 12:57 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

Dear members

We have typical vessel (site assembly), where backing gas arrangement could not be done for a stainless steel joint due to Safety (confined space), as well as space constraint.

One of the options will be using flux cored wire for GTAW.

Please share your view on these consumables for root pass of GTAW Stainless steel; where backing gas application is impractical, any body used these consumables?

Kobleco is manufacturing these wires under TGX series, any other manufactures who has similar product for this application?










--
SUPERTECH SERVICES LTD
Plot A-253, Road 30B,
Wagle Indl Estate,
Thane W 400 604
Maharashtra, India
Tel: +91-22-25826190/91
Fax: +91-22-25826189
Email: vdm@supertechservices.in
Web: www.supertechservices.in

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...