Dear Mr Mritunjay
 
Killed steel oxidised by addition of oxidizing agend to reduce oxigen content up to certail level to reduce any re4action during solidification.
 
Semi Killed steel is incompletly deoxidised and containing sufficient oxygen and during solidification it produce carbon monooxide.

On Mon, Sep 28, 2009 at 1:37 PM, Mrityunjay Kumar / ZS Saudi PEB QA/QC <Mrityunjaykumar@zamilsteel.com> wrote:

Dear all,
Can anybody tell me the difference between semi Killed & killed steel.

 Thanks and Regards,
M.K.Choudhary

     PEB - QA/QC
P.O. Box 877, Dammam 31421
Kingdom of Saudi Arabia
   +966 38471840 Ext- 555
    +966 38471840 Ext-559
 www.zamilsteel.com


--------------------------------------------------------------------------------------------------------
Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use, disseminate,
distribute, copy or alter this email. Any views or opinions presented in this
email are solely those of the author and might not represent those of "Zamil
Industrial" and or its units.

Warning: Although reasonable precautions have been taken to ensure no viruses
are present in this email, the company cannot accept responsibility for any
loss or damage arising from the use of this email or attachments. If you have
received this electronic mail message in error, please contact the sender directly.


--
Israr Ahmed Noor Mohammed
+966530417332

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...