[MW:3376] Re: Electrode for LTCS A333Gr6

Dear Kaushik,
 
SA 333 Gr 6 is generally recommended upto -46 deg C so you can use E7010 for root pass & E7018-1 for filling & capping or for better control you can also use GTAW root
 
Amarjit singh

On Mon, Sep 28, 2009 at 5:58 PM, checks patel <checkspatel@gmail.com> wrote:
Dear All,
 
I have a U/G pipeline of ASTM A 333 Gr.6 (LTCS) for 2 KM.
 
Which Electrode I can use for root pass and other pass and with which techniqe.
 
 
Regards,
 
Kaushik





--
Amarjit Singh

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...