Dear Mr. Choudhary,
Find below definitions fyi.

Killed steel: Completely deoxidized.
Semikilled: Not Completely deoxidized
Rimmed Steel: No deoxidizer added

Regards,
Rupesh Jambhale

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mrityunjay Kumar / ZS Saudi PEB QA/QC
Sent: 28 September 2009 16:07
To: materials-welding@googlegroups.com
Subject: [MW:3344] RE: 3331] Re: Base Metal


Dear all,
Can anybody tell me the difference between semi Killed & killed steel.

Thanks and Regards,
M.K.Choudhary

PEB - QA/QC
P.O. Box 877, Dammam 31421
Kingdom of Saudi Arabia
'   +966 38471840 Ext- 555
7    +966 38471840 Ext-559
ý   www.zamilsteel.com

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...