Hi!
Can anyone please guide me in welding of super duplex stainless steels UNS S32750.Or is it possible i can get a sample WPS.Also please let me know what all test are required to qualify PQR as Per ASME Sec IX:
1)Apart from tensile testing, bend testing
Coupons thickness :16 Inch Sch 40 S (9.56 mm)
Process:GTAW & SMAW

MDMT: -29 degrees to 170 degree C
Preheat temp?
Max.Interpass temp?
Sour service
Is ferritic test required?
PWHT?
Impact test:Please advise the locations of impact:Is HAZ/WCL/FL for the whole process is required or is it required seperately for Gtaw & SMAW process.

Appreciate if anyone could reply to me at the earliest.
Thanks & Regards,
Vipin george
Specilaist services,
Dubai,UAE

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

1 comment:

HLUSN8 said...

I can help you out. I have qualified procedure for uns 32750, with all testing including ferrite. We are a 'U' stamp shop. Drop me a line if you still need help. nramsli@cogeco.ca