Saturday, September 26, 2009

[MW:3330] Re: Painting

Hi Saravanan,

Please verify and check the following.

1. Check the amount of solvent for final coating.
2.Verify the over coating interval as per the paint manufacturer.
3.Check the mixing of coating materials.( for 5gal and above required mech stirrer).
4. Check the surface condistion of the base metal.

These are the probable reason, which may i am thinking. If the problem still exist, get the advice from paint manufacturer.

Regards,
M.R.Pramodh


--- On Sat, 9/26/09, Saarinen Mohan <sardev@gmail.com> wrote:

From: Saravanan Mohan <sardev@gmail.com>
Subject: [MW:3324] Painting
To: materials-welding@googlegroups.com
Date: Saturday, September 26, 2009, 2:16 PM

Dear Guys!!!!!!!
 
The project which I am involved following the paint systems as per client spec follows:-
 
Inorganic Zinc(75-100 micron) as a primer
High Build Epoxy(100-150 micron) as a Intermediate
High Solid Aliphatic Polyurethane(40-100 micron) as a finish
 
Total Dft between (215-350 micron)
 
After the complete curing of the finish coat visually I observed tiny pinholes like appearance or fish eye only inspector eye can find them.
 
Please give me the suggestion where the problem from? this appear in almost all the painted works which applied many different days, different paint batch followed by airlesspray method.
 
 
 
 




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...