We had similar problem after we fabricated Silicon Aluminium (SiAl) painted parts.

Silicon caused tiny holes on surface.

 

Good Luck!!

 

Tansu Ozcelebi
tansu@kreamakina.com
 

(*) KREA has been certified to ISO EN 3834-2:2005
(*)
www.kreamakina.com
(**) We are moved to new location.
Address and telephones are changed!!


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Saravanan Mohan
Sent: Saturday, September 26, 2009 11:46 AM
To: materials-welding@googlegroups.com
Subject: [MW:3324] Painting

 

Dear Guys!!!!!!!

 

The project which I am involved following the paint systems as per client spec follows:-

 

Inorganic Zinc(75-100 micron) as a primer

High Build Epoxy(100-150 micron) as a Intermediate

High Solid Aliphatic Polyurethane(40-100 micron) as a finish

 

Total Dft between (215-350 micron)

 

After the complete curing of the finish coat visually I observed tiny pinholes like appearance or fish eye only inspector eye can find them.

 

Please give me the suggestion where the problem from? this appear in almost all the painted works which applied many different days, different paint batch followed by airlesspray method.

 

 

 

 



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...