[MW:2599] RE: 2588] Temperbead WPS Qualification

Pl refer QW-290 of ASME Sec IX (2007) for Temper bead Welding and its
requirement.

Regards,
Vasanth

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Minal
Sent: 29 June 2009 19:58
To: Materials & Welding
Subject: [MW:2588] Temperbead WPS Qualification


I writing WPS that will include a Temperbead Tech, Preparing a set to
test WPS at the shop Facilities using
28 inch runpipe with 6 to 8 inch brach. What kind of mechanical tesing
shall be expected, if the code of construction will be ASME Sec.8 Div
1?
i know there will be a hardness test, any other help some pne can give
me idea to test?

Thanks in advance,
Minal

*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...