Monday, June 29, 2009

[MW:2586] Re: 2583] welding rod selection for dissimilarmaterials

Using the below mentioned welding consumables with proper preheat on P22 side does not even require PWHT .

Best Regards,
Francis Lobo
----- Original Message -----
From: Vasanthan Chandra (Lagos) <Vasanthan.Chandra@DeltaAfrik.com>
To: materials-welding@googlegroups.com
Sent: Mon, 29 Jun 2009 19:02:34 +0530 (IST)
Subject: [MW:2585] RE: 2583] welding rod selection for dissimilar materials

Ni alloy electrode can be used Like GTAW- ERNiCrMo-3, SMAW - ENiCrMo-3.


Regards,
Vasanth

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Srinivas
Sent: 29 June 2009 14:12
To: Materials & Welding
Subject: [MW:2583] welding rod selection for dissimilar materials


Dear all,

kindly let me know which welding filler wire &
welding rod can be used for A335 Gr.P 22 to S.S 316 materials

Thank you.

Srinivas

*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."


--
Click for exclusive coverage on the Maruti Ritz by ZigWheels.com experts
http://www.zigwheels.com/maruti-ritz?utm_source=mail&utm_medium=1&utm_content=ritz&utm_campaign=1

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...