depending on the code that will range from every project they need to be
required to every 5 years to never expired,
Original Message:
-----------------
From: sandy kumar sandy001987@gmail.com
Date: Mon, 29 Jun 2009 09:58:09 +0530
To: materials-welding@googlegroups.com
Subject: [MW:2565] lifetime of a qualified WPS
Can anyone tell whats is the validity period of a qualified WPS?
--------------------------------------------------------------------