As per B31.3, for 106Gr B up to 25mm thickness, no impact required with MDMT 0 Deg.C. For WPHY 65 is concerned, up to 15mm no impact is required.

Regards,
Vasanth

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of israr
Sent: 21 June 2009 06:45
To: Materials & Welding
Subject: [MW:2500] Re: Impact Test Requirements- ANSI


Dear Galagara,
I dont know about ANSI B31.1,3 and 4 but as per asme div-1 impact is
not required below 6mm thickness and material P1 up to operating
tempreture -29 degree celcius.

Israr Ahmed
+966530417332

On May 5, 2:59 am, "G.Alagarasan" <galagara...@rediffmail.com> wrote:
> Gents,
>
> Is impact testing required for below material as per ANSI 31.1,31.3,31.4 or any
>
> 1) MSS-SP75-WPHY 65 ( Weld o let) - P1 Gr 2 Material
>
> 2) SA 106 Gr B - P1 Gr 2 Material
>
> Thickness is 2.55mm,5.5mm and 13.5mm
>
> MDMT 0 Deg C
>
> Regards,
> Alagu


*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...