[MW:2591] Re: Formula to measure tensile

Dear Zoel,
Its load/Area of cross section.
Thanks,
Rajagopal

 
On 6/29/09, Zulfan Syahrian <z.syahrian@gmail.com> wrote:
Dear All,
 
anybody can advice me formula to get ultimate tensile strength in Ksi?,if test specimen have thickness 24.60mm,wide 20.36mm and ultimate tensile load 284.29KN
 