[MW:2527] Re: INCONEL CLAADING ON AUSTENITIC SS

inconel is relatively highcost material.Hence to save cost cladding is done.

On Sun, Jun 21, 2009 at 2:23 PM, somu <skmahalik@gmail.com> wrote:

DEAR SIR

PLEASE CLEAR MY DOUBTS WHICH ARE GIVEN BELOW..

1) WHY SS IS CLADDED WITH INCONEL? (LIKE INCONEL 625 ON SA240 TP 304L)

2) ITS PRACTICAL APPLICATIONS!!!

3) REASONS OF CRACKING -
                               - CENTRE LINE (BEAD) CRACKING IN CASE
OF STRIP CLADDING AND INCONEL JOINT


THANKING YOU

S.MAHALIK
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...