[MW:2528] Re: Joint category

Yes, all nozzle to shell joints are category D welds.
 
There are many types of category D welds.
1) Category D groove welds - when nozzle is either set-on or set-in type.
2) Category D butt welds- when nozzle is having lip type ends..
3) Category D fillet welds- when nozzle to shell weld is fillet welded without full penetration.
arun
On Wed, Jun 24, 2009 at 4:43 PM, amje <amolgengaje@gmail.com> wrote:
all nozzle to shell joints r always catagory d.


On Tue, Jun 23, 2009 at 7:17 PM, Arunachalam A <arunvani@gmail.com> wrote:
The following are the Code requirements for Category D butt welds:
 

UW-11 RADIOGRAPHIC AND ULTRASONIC EXAMINATION

(a) Full Radiography.

The following welded joints shall be examined radiographically for their full length in the

manner prescribed in UW-51:

(5)

all Category A and D butt welds in vessel sections and heads where the design of the joint or part is based

on a joint efficiency permitted by UW-12(a), .....

 
Nozzle size does not come into picture here. The butt joints need to be RTed depending on weld efficiency.
 
arun


On Mon, Jun 22, 2009 at 10:52 PM, G Padmanabhan <gpadmana@gmail.com> wrote:
Hi,
I agree with Category D joints.but RT requirements depends upon
eithere nozzle size or service condition requirements.

On Mon, Jun 22, 2009 at 4:42 PM, Arunachalam A <arunvani@gmail.com> wrote:
It is called catagory D butt weld, with RT requirements.
 
arun

On Mon, Jun 22, 2009 at 12:33 PM, Muhammed Ibrahim <ibratech@gmail.com> wrote:
Hi gents,
 
What is the joint category for lip type nozzle to shell weld?. Since it is butt weld is it include in Category A?. Sec. Viii shows the sketch of joint category nozzle to shell as cat. D.

--
Thanks & Regards
Muhammed Ibrahim PK





--
ARUNVANI

Smiling Opens the Heart

Good feelings for others are like ointments that heal wounds and re-establish friendships and relationships. Good feelings are generated in the mind, are transmitted through your attitude and are reflected in your eyes and smile. Smiling opens the heart and a glance can make miracles happen.

SMILE IS A COOLING SYSTEM OF HEART,
SPARKLING SYSTEM OF EYES, LIGHTING SYSTEM OF FACE, RELAXING SYSTEM OF MIND....
SO TO ACTIVATE ALL YOUR SYSTEM
==ALWAYS KEEP SMILING==





--
With Warm regards,

G.Padmanabhan
00967771103169





--
ARUNVANI

Smiling Opens the Heart

Good feelings for others are like ointments that heal wounds and re-establish friendships and relationships. Good feelings are generated in the mind, are transmitted through your attitude and are reflected in your eyes and smile. Smiling opens the heart and a glance can make miracles happen.

SMILE IS A COOLING SYSTEM OF HEART,
SPARKLING SYSTEM OF EYES, LIGHTING SYSTEM OF FACE, RELAXING SYSTEM OF MIND....
SO TO ACTIVATE ALL YOUR SYSTEM
==ALWAYS KEEP SMILING==








--
ARUNVANI

Smiling Opens the Heart

Good feelings for others are like ointments that heal wounds and re-establish friendships and relationships. Good feelings are generated in the mind, are transmitted through your attitude and are reflected in your eyes and smile. Smiling opens the heart and a glance can make miracles happen.

SMILE IS A COOLING SYSTEM OF HEART,
SPARKLING SYSTEM OF EYES, LIGHTING SYSTEM OF FACE, RELAXING SYSTEM OF MIND....
SO TO ACTIVATE ALL YOUR SYSTEM
==ALWAYS KEEP SMILING==

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...