Dear Monica,
You can use TIG (GTAW) or MIG (GMAW) methode and filler metal with AWS code ERCu
C7(Copper filler metal, tin-alloyed with good flow properties), gas: Argon-Helium, preheat to exclude discontiniuties..
regards,
Arjan
> Date: Wed, 24 Jun 2009 07:11:36 -0700
> Subject: [MW:2529] copper
> From: raphaelriccio@gmail.com
> To: materials-welding@googlegroups.com
>
>
> Hi,
>
> I have a big copper statue (monument) that i need to repair. which is
> the best welding?
>
> thanks,
> monica
>
> --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment