Dear Friends,

I am trying to weld IS2062 plate to a big EN19 rod as a spline. I am using ER7018 electrode. The preheating is done to 250 deg C of base and the welded plate. The welding is done in 1G position. When welding is finished it is heat treated at 630 deg C for 30 minutes as post weld heat treatment. But still I experience cracks in the parent material after welded portion cools down to room temperature.
Please suggest me some better solution to this process.

Regards,
Sachin Joshi


ICC World Twenty20 England '09 exclusively on YAHOO! CRICKET --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...