[MW:2505] Re: KSC42W

>
> Hi !
If it is maint. repair, you can get the consumables of L&T eutectic,Ador
Fontech,Magna make . which have a product of welding unknown material.
Only to be confirmed whether it is NF or Ferrous
You can check the chemistry by PMI machine

Regards

Hegde P.B.


I have to do some build up/repair work on KSC42W but I don't know what
> type of base material KSC42W is and the only thing I can find on the
> web describes the component it's used in, not the material
>
> http://translate.google.com/translate?hl=en&sl=ja&u=http://www.mesco-cast.co.jp/mesco/product/ship/ship.htm&ei=4-w6Srf8EYvW6gOblqGvDg&sa=X&oi=translate&resnum=1&ct=result&prev=/search%3Fq%3DKSC42W%26hl%3Den%26safe%3Doff%26rlz%3D1T4GGLJ_enSG318SG318
>
> Has anyone worked with this material before?
>
> >
>


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...