Skip to main content

[MW:2571] RE: 2567] Help Needed in Brazing

Hi!

I could not open the file but For lap joint  when two strips are to be joined some time vacuum brazing are carried with thin sheath is used as a filler ,  and this passes peel test

Regards

 

Hegde

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sachin Joshi
Sent: Monday, June 29, 2009 10:16 AM
To: materials-welding@googlegroups.com
Subject: [MW:2567] Help Needed in Brazing

 

Dear Sir,

We are having some difficulty in coming to common grounds with our customer on interpretation of ASME Section 9 qualification requirements for Copper to Copper lap joint with filler metal. I will try to explain you the entire case for your perusal and advice.
We are in the business of large motors for cement plants, generators and similar applications. The customer asks for qualification of operators in welding and brazing as per ASME section 9. The entire details of the joint are as attached in the document.
As per our interpretation of code the code asks for Tension test, Peel test and Section test. We get the tests done in approved authorised laboratories.
In all the tests the trend is such that the brazing coupons are passing in tensile tests and sectioning tests.
But the Peel test coupons does not have consistency in qualifying as per norms. As per the qualification criteria the test are basically visual inspection and have some inbuilt subjectivity hence the dispute keeps on recurring about the consistency of qualification.
In the clause QB-141.4 its is suggested that if the filler metal used has a greater strength than the base metal strength ( in out case UTS of base metal is 205 N/sq.mm, and filler metal UST is 250 N/sq mm) then the Peel test can be replaced with sectioning test. The customer is not agreeable as he feels that we are finding escape route by pointing to this clause.

Can you please throw some light on this issue with technical details of this substitution of peel test with sectioning test.

Kindly revert.

Regards,
Sachin Joshi

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...