'Grinding flush' of reinforcement depends of clients. If the vessel is designed for fatigue, then all the welds should have smooth contours.
arun

On Wed, Jun 24, 2009 at 10:33 AM, tong tong <tong2je@gmail.com> wrote:
UW-35 was referred but i don't understand what its mean. Can you explain to me..Thank

On Wed, Jun 24, 2009 at 2:03 PM, Ali Varmazyar <av-ssg@msa.ir> wrote:

Please see UW-35

 

Best Regards

 

A.V. 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of tong tong
Sent: Wednesday, June 24, 2009 9:40 AM
To: materials-welding@googlegroups.com
Subject: [MW:2518] Grind Flush

 

Dear All

I really need your help. It is true all weld reinforcement for high pressure vessel shall be grinded flush?. What code and standard should i refer? Thank in advance for your cooperation

Regards

Tong2je










--
ARUNVANI

Smiling Opens the Heart

Good feelings for others are like ointments that heal wounds and re-establish friendships and relationships. Good feelings are generated in the mind, are transmitted through your attitude and are reflected in your eyes and smile. Smiling opens the heart and a glance can make miracles happen.

SMILE IS A COOLING SYSTEM OF HEART,
SPARKLING SYSTEM OF EYES, LIGHTING SYSTEM OF FACE, RELAXING SYSTEM OF MIND....
SO TO ACTIVATE ALL YOUR SYSTEM
==ALWAYS KEEP SMILING==

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...