[MW:2569] Fw: [MW:2566] Re: lifetime of a qualified WPS


Dear Mr.Raghuram

If code changes after some years & there is a change in essential/supplementary essential variables, the wps will be valid.

regards

P.Kataiah


----- Forwarded by Kataiah/BelleliSA on 29/06/2009 07:44 ص -----
"BR" <raghurambathula@gmail.com>
Sent by: materials-welding@googlegroups.com

29/06/2009 07:37 ص
Please respond to materials-welding

       
        To:        "Materials & Welding" <materials-welding@googlegroups.com>
        cc:        
        Subject:        [MW:2566] Re: lifetime of a qualified WPS




None, yes its forever as long as it represents your production weld.
However changes may be made in the nonessential variables of a WPS to
suit production requirements without requalification provided such
changes are documented with respect to the essential, nonessential,
and, when required, supplementary essential variables for each
process. This may be by amendment to the WPS or by use of a new WPS.
Changes in essential or supplementary essential (when required)
variables require requalification of the WPS (new or additional PQRs
to support the change in essential or
supplementary essential variables).

On Jun 29, 8:28 am, sandy kumar <sandy001...@gmail.com> wrote:
> Can anyone tell whats is the validity period of a qualified WPS?

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...