[MW:2513] Brine Tank Material Selection

I have an old carbon steel brine tank which is severly corroded and
needs to be replaced. The brine solution contains ~ 10% salt (NaCl)
and 1% caustic (NaOH) at 110 deg F. The tank is used intermittently in
a batch process: filled for a few hours then drained and left empty
for 2 days. It is open to the atmosphere.

Initialy I was considering using 316 SS, but have been reading that
pitting could be a problem with the chloride. What material should be
used in this application?

Thanks for your help.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...