Hi,
That is if you do heat treatment of your PQR Test coupon to 80 minutes soaking time, then you can write a WPS for production welds to the maximum of 100 minutes soaking time.
Thanks,
K.Rajagopal
 
On 6/27/09, Jamie Welding <jamesmathewtrading@gmail.com> wrote:

Hi folks,
Can any one of u interpret the QW 407.3.
Especially the part PQR should be at least 80% aggregate times that in
production welds.




--
ARUNVANI

Smiling Opens the Heart

Good feelings for others are like ointments that heal wounds and re-establish friendships and relationships. Good feelings are generated in the mind, are transmitted through your attitude and are reflected in your eyes and smile. Smiling opens the heart and a glance can make miracles happen.

SMILE IS A COOLING SYSTEM OF HEART,
SPARKLING SYSTEM OF EYES, LIGHTING SYSTEM OF FACE, RELAXING SYSTEM OF MIND....
SO TO ACTIVATE ALL YOUR SYSTEM
==ALWAYS KEEP SMILING==

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...