I am looking for information on the chemical composition of Russia's
Black Steels in the following categories:

Steel Ст3 GOST 380-88

Steel Ст45 GOST 1050-88

Steel Ст20 GOST 1050-88

Thanks!

__________ Information from ESET NOD32 Antivirus, version of virus signature
database 4171 (20090619) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...